| General | |
|---|---|
| Material quality | iron |
| Product type | Gear |
| Powder pretreatment | Mix |
| Powder preparation method | Atomization method |
| Forming method | Compression molding |
| Mold material | Hard alloy die |
| Mold type | Die pressing |
| Sintering method | Solid-phase sintering |
| Sintering atmosphere | Decompose ammonia |
| Sintering temperature | 1050-2000. |
| Suppression method | Bidirectional molding |
| Post-processing | Heat treatment |
| Sampling cycle | 8 to 15 days |
| Processing cycle | 8 to 15 days |
| Annual processing capacity | 5000000 |
| Annual remaining processing capacity | 5000000 |
| Brand | "Lingyue" |
| Whether to process and customize | is |
| Whether to provide a design plan | is |
| Processing and customization | is |
| Processing method | Processing based on samples |